Nikel kaliteleri ve kimyasal bileşim
| saf nikel sınıfı | Ni+Co | Cu | Si | Mn | C | Mg | S | Fe | safsızlıklar toplamı | UNS tanımı |
| daha az olmayan | ||||||||||
| N2 | 99.98 | 0.001 | 0.003 | .002 | .005 | .003 | .001 | .007 | .02 | |
| N4 | 99.9 | 0.015 | 0.03 | .002 | .01 | .01 | .001 | .04 | 0.1 | N02201 |
| N6 | 99.5 | 0.06 | 0.10 | .05 | .10 | .10 | .005 | .10 | 0.5 | N02200 |
| N8 | 99.0 | 0.15 | 0.15 | .20 | .20 | .10 | .015 | .30 | 1.0 | |
| DN | 99.35 | 0.06 | 0.02-0.10 | 0.05 | .02.10 | .02-.10 | .005 | .10 | 0.35 | |
| NY1 | 99.7 | 0.1 | 0.1 | - | .02 | .10 | .005 | .10 | 0.3 | |
| NY2 | 99.4 | 0.01-0.10 | 0.1 | - | - | - | 0.002-0.01 | .10 | 0.6 | |
| NY3 | 99.0 | 0.15 | 0.2 | - | 0.1 | 10 | 0.005 | .25 | 1.0 | |
| NMg0.1 | 99.6 | 0.05 | 0.02 | .05 | .05 | 0.07~0.15 | 0.005 | .07 | .40 | |
| NSI0.19 | 99.4 | 0.05 | 0.15~0.25 | .05 | .10 | .05 | 0.005 | .07 | .50 | |
Nikelin korozyon direnci
Nikel, özellikle alkali korozyonuna karşı dirençlidir ve yüksek sıcaklıkta veya alevle eriyen alkalide nispeten kararlıdır, bu nedenle esas olarak alkali endüstrisinde kullanılır. Normal sıcaklıkta, salyangoz deniz suyunda, tuz çözeltisinde ve organik ortamda (yağ asidi, fenol, fermantasyon, vb.) son derece kararlıdır ve inorganik asit korozyonuna karşı dirençli veya asetik asit ve hafif asitte kararlı değildir.